Test methods for industrial sodium tripolyphosphate
工业三聚磷酸钠试验方法
Issue date: 2026-09-28 Implementation date: 2027-01-01
Issued by the General Administration of Quality Supervision, Inspection and Quarantine of the People's Republic of China
the Standardization Administration of the People's Republic of China
Contents
Foreword
1 Scope
2 Normative references
3 Terms and definitions
4 Preparation of test samples
5 Determination of whiteness
6 Determination of total phosphorus pentoxide content (quinoline phosphomolybdate gravimetric method)
7 Determination of different forms of phosphate
8 Determination of water-insoluble matter
9 Determination of loss on ignition
10 Determination of iron content
11 Determination of pH
12 Determination of particle size
13 Determination of apparent density
14 Determination of nitrogen oxide content (3,4-xylenol spectrophotometric method)
15 Determination of Type I content
16 Requirements for test result reports
Annex A (informative) Typical chromatogram of chromatographic separation
Test methods for industrial sodium tripolyphosphate
1 Scope
This document describes the test methods for 11 indicators of industrial sodium tripolyphosphate, including whiteness, total phosphorus pentoxide content, different forms of phosphate, water-insoluble matter, loss on ignition, iron content, pH, particle size, apparent density, nitrogen oxide content, and Type I content.
This document is applicable to the determination of industrial sodium tripolyphosphate. The determination of sodium pyrophosphate and sodium trimetaphosphate may refer to this document.
2 Normative references
The following documents, in whole or in part, are normatively referenced in this document and are indispensable for its application. For dated references, only the edition cited applies. For undated references, the latest edition (including any amendments) applies.
GB/T 3049, Chemical products for industrial use — General method for determination of iron content — 1,10-Phenanthroline spectrophotometric method
GB/T 6003.1, Test sieves — Technical requirements and testing — Part 1: Test sieves of metal wire cloth
GB/T 6682, Water for analytical laboratory use — Specification and test methods
GB/T 9086, Standard white plates for colorimetry and photometry
GB/T 13173, Surface active agents — Detergent test methods
JJG 512, Verification regulation for whiteness meters
3 Terms and definitions
For the purposes of this document, the following terms and definitions apply.
3.1
whiteness
The ratio of the diffuse reflected radiation of the surface of an object to that of a completely white (standard white) object in the visible region.
Note: Whiteness is expressed as a percentage.
3.2
apparent density
The mass per unit apparent volume.
3.3
Type I
A crystal form of industrial sodium tripolyphosphate formed by a different internal atomic arrangement within the crystal, characterized by relatively higher thermal stability and hygroscopicity.
3.4
Type II
Another crystal form of industrial sodium tripolyphosphate formed by a different internal atomic arrangement within the crystal, characterized by relatively lower thermal stability and hygroscopicity.
4 Preparation of test samples
The test sample shall be reduced to a certain quantity (500 g or more) for use in accordance with the sampling method for powder samples specified in GB/T 13173.
5 Determination of whiteness
5.1 Apparatus
5.1.1 Standard white plate
A standard white plate complying with GB/T 9086, used for calibrating the whiteness meter.
5.1.2 Working white plate
For convenience of measurement, a white ceramic plate with a smooth, scratch-free and crack-free surface may be used as the working white plate for daily whiteness measurement. The working white plate shall be calibrated monthly using the standard white plate. The working white plate shall be stored in a desiccator in a dark place. If contaminated, it shall be wiped clean with a soft cloth or degreased cotton dipped in anhydrous ethanol. It shall then be placed in a drying oven at 105 °C to 110 °C for 30 min, removed, and placed in a desiccator to cool to room temperature before being calibrated with the standard white plate.
5.1.3 Whiteness meter
The optical geometry of the instrument may be any of the following: perpendicular/vertical (o/d), diffuse/vertical (d/o), 45°/vertical (45°/o) or vertical/45° (o/45°). The light source of the instrument may be a D65 or C light source. The reading accuracy of the instrument shall reach the first decimal place. The instrument shall meet the requirements of Grade II or above in JJG 512.
5.2 Test procedure
5.2.1 Turn on, preheat and adjust the instrument according to the instruction manual.
5.2.2 Select an appropriate sample quantity according to the density of the test sample and the size of the powder press, and press it into a test plate with a smooth surface, free from cracks and stains in accordance with the procedures specified in GB/T 9086. Two test plates shall be pressed simultaneously for each test.
Note: When using the HY-3 powder press, the sample quantity is 9 g.
5.2.3 Calibrate the instrument to display a stable standard value using the standard white plate or the working white plate.
5.2.4 After the instrument has been calibrated and stabilized, measure and record the three stimulus values XX, YY, and ZZ for each test plate.
5.3 Calculation of results
5.3.1 This document adopts the whiteness formula recommended by the International Commission on Illumination (CIE) in 1986 for calculating whiteness [see Formula (1) and Formula (2)], and shall be used in conjunction with the chromaticity difference formula [see Formula (3) and Formula (4)].
Standard
GB/T 9984-2026 Test methods for industrial sodium tripolyphosphate (English)
Standard No.
GB/T 9984-2026
Status
to be valid
Language
English
File Format
PDF
Word Count
17500 words
Translation Price(USD)
525.0
Implemented on
2027-4-1
Delivery
via email in 1~5 business day
Detail of GB/T 9984-2026
Standard No.
GB/T 9984-2026
English Name
Test methods for industrial sodium tripolyphosphate
GB/T 9984-2026 Test methods for industrial sodium tripolyphosphate English, Anglais, Englisch, Inglés, えいご
This is a draft translation for reference among interesting stakeholders. The finalized translation (passing through draft translation, self-check, revision and verification) will be delivered upon being ordered.
ICS
CCS
National Standard of the People's Republic of China
GB/T 9984-2026
Test methods for industrial sodium tripolyphosphate
工业三聚磷酸钠试验方法
Issue date: 2026-09-28 Implementation date: 2027-01-01
Issued by the General Administration of Quality Supervision, Inspection and Quarantine of the People's Republic of China
the Standardization Administration of the People's Republic of China
Contents
Foreword
1 Scope
2 Normative references
3 Terms and definitions
4 Preparation of test samples
5 Determination of whiteness
6 Determination of total phosphorus pentoxide content (quinoline phosphomolybdate gravimetric method)
7 Determination of different forms of phosphate
8 Determination of water-insoluble matter
9 Determination of loss on ignition
10 Determination of iron content
11 Determination of pH
12 Determination of particle size
13 Determination of apparent density
14 Determination of nitrogen oxide content (3,4-xylenol spectrophotometric method)
15 Determination of Type I content
16 Requirements for test result reports
Annex A (informative) Typical chromatogram of chromatographic separation
Test methods for industrial sodium tripolyphosphate
1 Scope
This document describes the test methods for 11 indicators of industrial sodium tripolyphosphate, including whiteness, total phosphorus pentoxide content, different forms of phosphate, water-insoluble matter, loss on ignition, iron content, pH, particle size, apparent density, nitrogen oxide content, and Type I content.
This document is applicable to the determination of industrial sodium tripolyphosphate. The determination of sodium pyrophosphate and sodium trimetaphosphate may refer to this document.
2 Normative references
The following documents, in whole or in part, are normatively referenced in this document and are indispensable for its application. For dated references, only the edition cited applies. For undated references, the latest edition (including any amendments) applies.
GB/T 3049, Chemical products for industrial use — General method for determination of iron content — 1,10-Phenanthroline spectrophotometric method
GB/T 6003.1, Test sieves — Technical requirements and testing — Part 1: Test sieves of metal wire cloth
GB/T 6682, Water for analytical laboratory use — Specification and test methods
GB/T 9086, Standard white plates for colorimetry and photometry
GB/T 13173, Surface active agents — Detergent test methods
JJG 512, Verification regulation for whiteness meters
3 Terms and definitions
For the purposes of this document, the following terms and definitions apply.
3.1
whiteness
The ratio of the diffuse reflected radiation of the surface of an object to that of a completely white (standard white) object in the visible region.
Note: Whiteness is expressed as a percentage.
3.2
apparent density
The mass per unit apparent volume.
3.3
Type I
A crystal form of industrial sodium tripolyphosphate formed by a different internal atomic arrangement within the crystal, characterized by relatively higher thermal stability and hygroscopicity.
3.4
Type II
Another crystal form of industrial sodium tripolyphosphate formed by a different internal atomic arrangement within the crystal, characterized by relatively lower thermal stability and hygroscopicity.
4 Preparation of test samples
The test sample shall be reduced to a certain quantity (500 g or more) for use in accordance with the sampling method for powder samples specified in GB/T 13173.
5 Determination of whiteness
5.1 Apparatus
5.1.1 Standard white plate
A standard white plate complying with GB/T 9086, used for calibrating the whiteness meter.
5.1.2 Working white plate
For convenience of measurement, a white ceramic plate with a smooth, scratch-free and crack-free surface may be used as the working white plate for daily whiteness measurement. The working white plate shall be calibrated monthly using the standard white plate. The working white plate shall be stored in a desiccator in a dark place. If contaminated, it shall be wiped clean with a soft cloth or degreased cotton dipped in anhydrous ethanol. It shall then be placed in a drying oven at 105 °C to 110 °C for 30 min, removed, and placed in a desiccator to cool to room temperature before being calibrated with the standard white plate.
5.1.3 Whiteness meter
The optical geometry of the instrument may be any of the following: perpendicular/vertical (o/d), diffuse/vertical (d/o), 45°/vertical (45°/o) or vertical/45° (o/45°). The light source of the instrument may be a D65 or C light source. The reading accuracy of the instrument shall reach the first decimal place. The instrument shall meet the requirements of Grade II or above in JJG 512.
5.2 Test procedure
5.2.1 Turn on, preheat and adjust the instrument according to the instruction manual.
5.2.2 Select an appropriate sample quantity according to the density of the test sample and the size of the powder press, and press it into a test plate with a smooth surface, free from cracks and stains in accordance with the procedures specified in GB/T 9086. Two test plates shall be pressed simultaneously for each test.
Note: When using the HY-3 powder press, the sample quantity is 9 g.
5.2.3 Calibrate the instrument to display a stable standard value using the standard white plate or the working white plate.
5.2.4 After the instrument has been calibrated and stabilized, measure and record the three stimulus values XX, YY, and ZZ for each test plate.
5.3 Calculation of results
5.3.1 This document adopts the whiteness formula recommended by the International Commission on Illumination (CIE) in 1986 for calculating whiteness [see Formula (1) and Formula (2)], and shall be used in conjunction with the chromaticity difference formula [see Formula (3) and Formula (4)].